Dow 500.00 Developmental Performance Polypropylene Polymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow 500.00 Developmental Performance Polypropylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
D 500.00 Developmental Performance Polymer is a performance plastic designed for cut sheet thermoforming. The propylene-based polymer offers improved formability in large part thermoforming applications.Main CharacteristicsMelt strength specifically suited to the thermoforming processImproved sheet sag / drape performanceLow temperature toughnessHigh chemical resistanceBetter regrind capability without significant loss of propertiesDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Melt Index of Compound 0.45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
Tangent; ASTM D790A
Izod Impact, Notched 1.07 J/cm

@Temperature -18.0 °C
2.00 ft-lb/in

@Temperature -0.400 °F
ASTM D256
5.87 J/cm

@Temperature 23.0 °C
11.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
Peak Energy; ASTM D3763
30.7 J

@Temperature -18.0 °C
22.6 ft-lb

@Temperature -0.400 °F
Peak Energy; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.3 °C
137 °F
Unannealed; ASTM D648
Optical Properties Metric English Comments
Gloss >= 80 %
>= 80 %
ASTM D523; 60°, Thermoformed
90 %
90 %
ASTM D523; 60°, Extruded Sheet