Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87564 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M4805 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5005 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req.. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa.. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -30.0 °C |
2.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
double-gated; SABIC Method |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -30.0 °C |
2.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXE173R PC This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
Practical Use; ASTM-D256 |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 285A2R30018 Cellulose Acetate Butyrate, Natural, Trsp Applications:OphthalmicsOptical safety framesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, cla.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTACARB 0820 GF V0-5V HF Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good melt flow rate, good processability, g.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1050 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 0.000 °C |
2.06 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1515 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood melt flow rate, good impact resistance, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tritan MX711 Copolyester Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -20.0 °C |
2.06 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 05100 GFC Polypropylene, 50% Glass Filled PP homopolymer 50% chemically coupled glass fiberExcellent stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 23.0 °C |
2.06 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 0560 HFC Polypropylene, 30% Glass Filled PP homopolymer 30% chemically coupled glass fiber reinforcedGood stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature 0.000 °C |
2.06 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 0580 GFC Polypropylene, 40% Glass Filled PP homopolymer 40% chemically coupled glass fiberExcellent stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.10 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
2.06 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -30.0 °C |
2.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -30.0 °C |
2.06 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Izod Impact, Notched | 1.10 J/cm @Temperature -40.0 °C |
2.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |