Polymer Property : Impact Test = 7.38 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp FX00617 PE
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific)
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia..
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66
LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO
LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su..
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific)
LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec..
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon EE005 PEI
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific)
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC
LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC
LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare.
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp JF003L PES
LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r..
Impact Test 10.0 J
7.38 ft-lb
Instrumented Dart Impact (Energy at Peak Force); ASTM Test
Styrolution Styrolux 3G55 SBC
Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex..
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6
LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC..
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 (Asia Pacific)
LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC..
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV006S PP
LNP* VERTON* MV006S is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Structural.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV006S PP (Asia Pacific)
LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV008S PP
LNP VERTON* MV008S is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV008S PP (Asia Pacific)
LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV008S PP (Europe-Africa-Middle East)
LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV008SU PP
LNP VERTON* MV008SU is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV008SU PP (Europe-Africa-Middle East)
LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized, UV-Stabilized.
Impact Test 10.0 J

@Temperature 23.0 °C
7.38 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE)
LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE
LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC
LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific)
LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding.
Impact Test 10.0 J
7.38 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP VERTON MV008SXP PP (Europe-Africa-Middle East)
LNP* Verton* MV008SXP is a compound based on Polypropylene resin containing Long Glass. Added features include: Chemically Coupled, Heat Stabilized.