Category | Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC |
Manufacturer | Styrolution |
Trade Name | Styrolux |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Styrolution Styrolux 3G55 SBC.pdf |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Water Absorption | 0.070 % | 0.070 % | ISO 62 |
Moisture Absorption at Equilibrium | 0.070 % | 0.070 % | 23°C/50% R.H.; ISO 62 |
Moisture Vapor Transmission | 1.70 cc-mm/m²-24hr-atm | 4.32 cc-mil/100 in²-24hr-atm | 100% RH; ASTM Test |
Oxygen Transmission Rate | 500 cc/m²/day | 32.2 cc/100 in²/day | 0% RH; ASTM Test |
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | ASTM Data; MD |
Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 200 °C |
15 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Test |
16 g/10 min @Load 5.00 kg, Temperature 200 °C |
16 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.0 MPa | 2320 psi | 2 in/min; ASTM Test |
20.0 MPa | 2900 psi | 50mm/min; ISO 527 | |
Elongation at Break | >= 50 % | >= 50 % | 50mm/min, Nominal strain; ISO 527 |
>= 300 % | >= 300 % | 2 in/min; ASTM Test | |
300 % | 300 % | 0.2 in/min; ASTM Test | |
Elongation at Yield | 2.0 % | 2.0 % | 50mm/min; ISO 527 |
Tensile Modulus | 0.900 GPa | 131 ksi | 1mm/min; ISO 527 |
1.17 GPa | 170 ksi | 2 in/min; ASTM Test | |
Flexural Strength | 17.0 MPa | 2470 psi | ASTM Test |
18.0 MPa | 2610 psi | ISO Data | |
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM Test |
0.900 GPa | 131 ksi | ISO Data | |
Secant Modulus, MD | 0.835 GPa | 121 ksi | ASTM Test |
Secant Modulus, TD | 0.685 GPa | 99.4 ksi | ASTM Test |
Izod Impact, Notched | NB @Thickness 3.17 mm |
NB @Thickness 0.125 in |
ASTM Test |
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO Test |
Charpy Impact Unnotched | NB | NB | ISO 179 |
8.70 J/cm² @Temperature -30.0 °C |
41.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 | |
Charpy Impact, Notched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO 179 |
0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 179 | |
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | ASTM Test |
Impact Test | 10.0 J | 7.38 ft-lb | Instrumented Dart Impact (Energy at Peak Force); ASTM Test |
Elmendorf Tear Strength MD | 830 g | 830 g | ASTM Data |
Elmendorf Tear Strength TD | 339 g | 339 g | ASTM Data |
Film Tensile Strength at Break, MD | 310 MPa | 45000 psi | ASTM Data |
Film Tensile Strength at Break, TD | 350 MPa | 50800 psi | ASTM Data |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359 |
CTE, linear, Transverse to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM Test |
Deflection Temperature at 0.46 MPa (66 psi) | 62.0 °C | 144 °F | ISO 75 |
67.0 °C | 153 °F | ASTM Test | |
Deflection Temperature at 1.8 MPa (264 psi) | 46.0 °C | 115 °F | ASTM Test |
51.0 °C | 124 °F | ISO 75 | |
Vicat Softening Point | 35.0 °C | 95.0 °F | (50 °C/h / 50N) - B/50; ISO 306 |
72.0 °C | 162 °F | Rate "B" Loading 1 (120 degC/h 10N); ASTM Test | |
Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
|
HB @Thickness 3.20 mm |
HB @Thickness 0.126 in |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.57 | 1.57 | ASTM Test |
Haze | 1.6 % @Thickness 3.20 mm |
1.6 % @Thickness 0.126 in |
ASTM Test |
Transmission, Visible | 90 % | 90 % |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
Dielectric Constant | 2.5 @Frequency 1e+9 Hz |
2.5 @Frequency 1e+9 Hz |
ASTM Data |
2.5 @Frequency 1.00e+6 Hz |
2.5 @Frequency 1.00e+6 Hz |
ASTM Data | |
2.5 @Frequency 100 Hz |
2.5 @Frequency 100 Hz |
IEC 60250 | |
2.5 @Frequency 1.00e+6 Hz |
2.5 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Dielectric Strength | 80.0 kV/mm | 2030 kV/in | IEC 60243-1 |
Dissipation Factor | 0.00030 @Frequency 1e+9 Hz |
0.00030 @Frequency 1e+9 Hz |
ASTM Data |
0.00030 @Frequency 100 Hz |
0.00030 @Frequency 100 Hz |
IEC 60250 | |
0.00080 @Frequency 1.00e+6 Hz |
0.00080 @Frequency 1.00e+6 Hz |
ASTM Data | |
0.00080 @Frequency 1.00e+6 Hz |
0.00080 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Extrusion |
180 - 250 °C | 356 - 482 °F | Injection Molding | |
230 °C | 446 °F | Injection molding | |
Mold Temperature | 30.0 - 50.0 °C | 86.0 - 122 °F | Injection Molding |
Injection Velocity | 50.0 mm/sec | 1.97 in/sec | Injection molding |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Clear | |
Commercial Status | Active America | |
FDA | Yes | |
Form | Yes | |
Impact Modified | Yes | |
NSF Std. 51 | No | |
NSF Std. 61 | No | |
Primary Processing Technique | Extrusion | |
Processing | Blow Molding | |
Film Extrusion | ||
Injection Molding | ||
Other Extrusion | ||
Sheet Extrusion | ||
UL.UL-C | No |