Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Impact Test | 11.0 J | 8.11 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DD0001I PC LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific) LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 11.0 J | 8.11 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON MD000AP PP LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific) LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific) LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 11.0 J | 8.11 ft-lb | Instrumented Dart Impact (Energy at Peak Force); ASTM Test |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp ZF008 PPO LNP* Thermocomp* ZF008 is a compound based on Modified PPO containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp 5C003 LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. Also known as THERMOCOMP* FP-VC.. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp DF0066P PC LNP THERMOCOMP* DF0066P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing.This data was supplied by.. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp XF006S LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.. |
|||
Impact Test | 11.0 J | 8.11 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East) LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Impact Test | 11.0 J | 8.11 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON MFD02 PP LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 11.0 J | 8.11 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific) LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 11.0 J | 8.11 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East) LNP VERTON* WV00A is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |