Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP VERTON* WV00A is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ASTM D 792
1.70 g/cc
0.0614 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.090 %
0.090 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00080 - 0.0029 cm/cm

@Time 86400 sec
0.00080 - 0.0029 in/in

@Time 24.0 hour
ISO 294
0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm

@Time 86400 sec
0.0040 - 0.0070 in/in

@Time 24.0 hour
ASTM D 955
0.0043 - 0.0072 cm/cm

@Time 86400 sec
0.0043 - 0.0072 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 154 MPa
22300 psi
ASTM D 638
163 MPa
23600 psi
ISO 527
Elongation at Break 1.0 %
1.0 %
ISO 527
1.1 %
1.1 %
ASTM D 638
Tensile Modulus 19.77 GPa
2867 ksi
1 mm/min; ISO 527
20.24 GPa
2936 ksi
50 mm/min; ASTM D 638
Flexural Strength 233 MPa
33800 psi
ASTM D 790
235 MPa
34100 psi
ISO 178
Flexural Modulus 14.4 GPa
2090 ksi
ASTM D 790
15.67 GPa
2273 ksi
ISO 178
Izod Impact, Unnotched 8.31 J/cm

@Temperature 23.0 °C
15.6 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 40.0 kJ/m²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
43.0 kJ/m²

@Temperature -40.0 °C
20.5 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 59.0 kJ/m²

@Temperature 23.0 °C
28.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 11.0 J
8.11 ft-lb
Multiaxial Impact; ISO 6603
12.0 J

@Temperature 23.0 °C
8.85 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
18.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 41.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
41.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
223 °C

@Thickness 3.20 mm
433 °F

@Thickness 0.126 in
unannealed; ASTM D 648