Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity Test = 140 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 140 - 150 cm³/g
140 - 150 cm³/g
Average value: 147 cm³/g Grade Count:4
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Viscosity Test 140 - 150 cm³/g
140 - 150 cm³/g
Average value: 147 cm³/g Grade Count:13
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Viscosity Test 140 - 150 cm³/g
140 - 150 cm³/g
Average value: 144 cm³/g Grade Count:9
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber
30% Glass fiber reinforced; injection molding grade
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Pocan® B 1501 000000 PBT
PBT, non-reinforced, injection molding, extrusion, food contact
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Pocan® B 1505 000000 PBT
PBT, non-reinforced, injection molding, extrusion
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity Number
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity Number
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Viscosity Test 140 cm³/g
140 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per..
Viscosity Test 140 cm³/g
140 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided ..
Viscosity Test 140 cm³/g
140 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66  (Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P..
Viscosity Test 140 cm³/g
140 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa..
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned)
Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry)
Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned)
Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade.
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Conditioned)
Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability.
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)
Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability.
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif..
Viscosity Test 140 cm³/g
140 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..
Viscosity Test 140 - 150 cm³/g
140 - 150 cm³/g
Average value: 148 cm³/g Grade Count:8
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Viscosity Test 140 cm³/g
140 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont ..
Viscosity Test 140 cm³/g
140 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade.
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number; ISO 307
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number
BASF Ultramid® B3WG6 BK00564 BGVW 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 BK00564 BGVW is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
Copyright © lookpolymers.com All Rights Reserved