Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
Water Absorption | 0.50 % | 0.50 % | Test Sim. to ISO 62 |
Moisture Absorption at Equilibrium | 0.20 % | 0.20 % | 23°C/50% R.H.; Test Sim. to ISO 62 |
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 260 °C |
20 g/10 min @Load 4.76 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 60.0 MPa | 8700 psi | ISO 527-1/-2 |
Elongation at Break | >= 50 % | >= 50 % | Nominal; ISO 527-1/-2 |
Elongation at Yield | 4.0 % | 4.0 % | ISO 527-1/-2 |
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
Charpy Impact Unnotched | 20.0 J/cm² @Temperature -30.0 °C |
95.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eU | |
Charpy Impact, Notched | <= 1.00 J/cm² @Temperature -30.0 °C |
<= 4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
<= 1.00 J/cm² @Temperature 23.0 °C |
<= 4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA | |
Impact | 3563 | 3563 | Puncture maximum force (N); ISO 6603-2 |
Puncture Energy | 43.0 J | 31.7 ft-lb | ISO 6603-2 |
Tensile Creep Modulus, 1 hour | 2200 MPa | 319000 psi | ISO 899-1 |
Tensile Creep Modulus, 1000 hours | 1300 MPa | 189000 psi | ISO 899-1 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359-1/-2 |
CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
Melting Point | 225 °C | 437 °F | 10°C/min; ISO 11357-1/-3 |
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75-1/-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ISO 75-1/-2 |
Deflection Temperature at 8.0 MPa | 45.0 °C | 113 °F | ISO 75-1/-2 |
Vicat Softening Point | 180 °C | 356 °F | 50°C/h 50N; ISO 306 |
Flammability, UL94 | HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
IEC 60695-11-10 |
HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
IEC 60695-11-10 | |
Oxygen Index | 24 % | 24 % | ISO 4589-1/-2 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | IEC 60093 |
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
Dielectric Constant | 3.2 @Frequency 1.00e+6 Hz |
3.2 @Frequency 1.00e+6 Hz |
IEC 60250 |
3.4 @Frequency 100 Hz |
3.4 @Frequency 100 Hz |
IEC 60250 | |
Dielectric Strength | 27.0 kV/mm | 686 kV/in | IEC 60243-1 |
Dissipation Factor | 0.0015 @Frequency 100 Hz |
0.0015 @Frequency 100 Hz |
IEC 60250 |
0.019 @Frequency 1.00e+6 Hz |
0.019 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
Mold Temperature | 80.0 °C | 176 °F | Injection Molding; ISO 10724 |
Descriptive Properties | Value | Comments |
---|---|---|
Additives | Release agent | |
Form | Pellets | |
ISO Shortname | ISO 7792-1-PBT,GR,11-030 | |
Processing | Injection molding | |
Region | Asia Pacific | |
Europe | ||
Near East/Africa | ||
North America | ||
South and Central America |