Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
Manufacturer | |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.33 g/cc | 0.0480 lb/in³ | DAM; ISO 1183 |
Water Absorption | 2.0 % @Temperature 23.0 °C |
2.0 % @Temperature 73.4 °F |
Equilibrium 50%RH; DAM; ISO 62, Similar to |
6.4 % @Temperature 23.0 °C |
6.4 % @Temperature 73.4 °F |
Saturation, immersed; DAM; ISO 62, Similar to | |
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 2.00 mm |
0.0030 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 87 | 87 | 50%RH; ISO 2039/2 |
103 | 103 | DAM; ISO 2039/2 | |
Hardness, Rockwell R | 116 | 116 | 50%RH; ISO 2039/2 |
123 | 123 | DAM; ISO 2039/2 | |
Tensile Strength at Break | 115 MPa @Temperature 23.0 °C |
16700 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
188 MPa @Temperature 23.0 °C |
27300 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
Elongation at Break | 3.1 % @Temperature 23.0 °C |
3.1 % @Temperature 73.4 °F |
DAM; ISO 527 |
5.0 % @Temperature 23.0 °C |
5.0 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
Tensile Modulus | 6.10 GPa @Temperature 23.0 °C |
885 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
8.60 GPa @Temperature 23.0 °C |
1250 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
Flexural Strength | 165 MPa @Temperature 23.0 °C |
23900 psi @Temperature 73.4 °F |
50%RH; ISO 178 |
240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
DAM; ISO 178 | |
Shear Modulus | 0.265 GPa @Temperature 250 °C |
38.4 ksi @Temperature 482 °F |
DAM; ISO 6721 |
0.348 GPa @Temperature 240 °C |
50.5 ksi @Temperature 464 °F |
DAM; ISO 6721 | |
0.395 GPa @Temperature 230 °C |
57.3 ksi @Temperature 446 °F |
DAM; ISO 6721 | |
0.426 GPa @Temperature 220 °C |
61.8 ksi @Temperature 428 °F |
DAM; ISO 6721 | |
0.448 GPa @Temperature 210 °C |
65.0 ksi @Temperature 410 °F |
DAM; ISO 6721 | |
0.464 GPa @Temperature 200 °C |
67.3 ksi @Temperature 392 °F |
DAM; ISO 6721 | |
0.479 GPa @Temperature 190 °C |
69.5 ksi @Temperature 374 °F |
DAM; ISO 6721 | |
0.495 GPa @Temperature 180 °C |
71.8 ksi @Temperature 356 °F |
DAM; ISO 6721 | |
0.510 GPa @Temperature 170 °C |
74.0 ksi @Temperature 338 °F |
DAM; ISO 6721 | |
0.524 GPa @Temperature 160 °C |
76.0 ksi @Temperature 320 °F |
DAM; ISO 6721 | |
0.539 GPa @Temperature 150 °C |
78.2 ksi @Temperature 302 °F |
DAM; ISO 6721 | |
0.556 GPa @Temperature 140 °C |
80.6 ksi @Temperature 284 °F |
DAM; ISO 6721 | |
0.575 GPa @Temperature 130 °C |
83.4 ksi @Temperature 266 °F |
DAM; ISO 6721 | |
0.597 GPa @Temperature 120 °C |
86.6 ksi @Temperature 248 °F |
DAM; ISO 6721 | |
0.628 GPa @Temperature 110 °C |
91.1 ksi @Temperature 230 °F |
DAM; ISO 6721 | |
0.676 GPa @Temperature 100 °C |
98.0 ksi @Temperature 212 °F |
DAM; ISO 6721 | |
0.754 GPa @Temperature 90.0 °C |
109 ksi @Temperature 194 °F |
DAM; ISO 6721 | |
0.878 GPa @Temperature 80.0 °C |
127 ksi @Temperature 176 °F |
DAM; ISO 6721 | |
1.05 GPa @Temperature 70.0 °C |
152 ksi @Temperature 158 °F |
DAM; ISO 6721 | |
1.29 GPa @Temperature 60.0 °C |
187 ksi @Temperature 140 °F |
DAM; ISO 6721 | |
1.60 GPa @Temperature 50.0 °C |
232 ksi @Temperature 122 °F |
DAM; ISO 6721 | |
1.72 GPa @Temperature 40.0 °C |
249 ksi @Temperature 104 °F |
DAM; ISO 6721 | |
1.78 GPa @Temperature 30.0 °C |
258 ksi @Temperature 86.0 °F |
DAM; ISO 6721 | |
1.83 GPa @Temperature 20.0 °C |
265 ksi @Temperature 68.0 °F |
DAM; ISO 6721 | |
1.87 GPa @Temperature 10.0 °C |
271 ksi @Temperature 50.0 °F |
DAM; ISO 6721 | |
1.90 GPa @Temperature 0.000 °C |
276 ksi @Temperature 32.0 °F |
DAM; ISO 6721 | |
1.91 GPa @Temperature -10.0 °C |
277 ksi @Temperature 14.0 °F |
DAM; ISO 6721 | |
1.92 GPa @Temperature -20.0 °C |
278 ksi @Temperature -4.00 °F |
DAM; ISO 6721 | |
1.93 GPa @Temperature -30.0 °C |
280 ksi @Temperature -22.0 °F |
DAM; ISO 6721 | |
1.96 GPa @Temperature -40.0 °C |
284 ksi @Temperature -40.0 °F |
DAM; ISO 6721 | |
1.99 GPa @Temperature -50.0 °C |
289 ksi @Temperature -58.0 °F |
DAM; ISO 6721 | |
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A | |
10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
11.0 kJ/m² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A | |
Charpy Impact Unnotched | 4.70 J/cm² @Temperature -30.0 °C |
22.4 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
5.30 J/cm² @Temperature -30.0 °C |
25.2 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU | |
8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU | |
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA | |
1.10 J/cm² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA | |
1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA | |
Tensile Creep Modulus, 1 hour | 5000 MPa @Temperature 23.0 °C |
725000 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
Tensile Creep Modulus, 1000 hours | 4100 MPa @Temperature 23.0 °C |
595000 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 23.0 °C |
1.00e+11 ohm-cm @Temperature 73.4 °F |
50%RH; IEC 60093 |
>= 1.00e+15 ohm-cm @Temperature 23.0 °C |
>= 1.00e+15 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 | |
1.00e+17 ohm-cm @Temperature 23.0 °C |
1.00e+17 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 | |
Surface Resistance | 1.00e+13 ohm @Temperature 23.0 °C |
1.00e+13 ohm @Temperature 73.4 °F |
50%RH; IEC 60093 |
>= 1.00e+15 ohm @Temperature 23.0 °C |
>= 1.00e+15 ohm @Temperature 73.4 °F |
DAM; IEC 60093 |