Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 220 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 220 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Melt Flow | 7.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
7.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 7.0 - 11 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 - 11 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond I; ASTM D1238 |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS6 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS6 PC (Asia Pacific) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® IR2840 PC 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXRL0662 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Kuraray SEPTON® S2063 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC0700 PC PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC0703R PC PC0703R resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market.This data was supplied by SABIC-IP f.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC0800 PC PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 250 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 265 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ABS 1950 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Terluran® HH-106 ABS Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Chi Mei Kibiton® PB-575 SBC Shoe sole industrial accessory |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 220 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 428 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Calsak CS-72L General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |
|||
Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 190 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Elastamax HTE 2101-1000 Polyurethane Alloy
(discontinued **) This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. .. |