| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | 0.125 in; ASTM D955 |
| Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
| 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond I; ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 110 | 110 | ASTM D785 |
| Tensile Strength, Yield | 46.2 MPa | 6700 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Tensile Modulus | 2.59 GPa | 375 ksi | ASTM D638 |
| Flexural Yield Strength | 75.8 MPa | 11000 psi | ASTM D790 |
| Flexural Modulus | 2.52 GPa | 365 ksi | ASTM D790 |
| Izod Impact, Notched | 2.40 J/cm | 4.50 ft-lb/in | 0.25 in; ASTM D256 |
| 2.67 J/cm | 5.00 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 101 µm/m-°C @Temperature -40.0 - 176 °C |
56.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
| Vicat Softening Point | 101 °C | 214 °F | ASTM D1525 |
| Flammability, UL94 | HB | HB | |
| V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 191 - 210 °C | 375 - 410 °F | |
| Middle Barrel Temperature | 210 - 229 °C | 410 - 445 °F | |
| Front Barrel Temperature | 221 - 249 °C | 430 - 480 °F | |
| Nozzle Temperature | 221 - 243 °C | 430 - 470 °F | |
| Melt Temperature | 257 °C | 495 °F | |
| Mold Temperature | 60.0 - 79.4 °C | 140 - 175 °F | |
| Moisture Content | <= 0.020 % | <= 0.020 % | |
| Injection Pressure | 4.83 - 6.89 MPa | 700 - 1000 psi | |
| Back Pressure | 0.483 - 0.965 MPa | 70.0 - 140 psi | |
| Shot Size | 40 - 80 % | 40 - 80 % | |
| Screw Speed | 50 - 90 rpm | 50 - 90 rpm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure | 550 to 850 psi | |
| Injection Rate | Slow |