Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.50 g/10 min @Load 1.00 kg, Temperature 235 °C |
0.50 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 7200 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 240 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 464 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
Melt Flow | 0.50 - 0.70 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.50 - 0.70 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6749F (486H6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.50 - 0.90 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.50 - 0.90 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PP 8332C (EPD60R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PE 1270
(discontinued **) PRE-ELEC PE 1270 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 12.. |
|||
Melt Flow | 0.50 - 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 - 0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4153L (524F6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg |
0.50 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Lacqtene® 2001 PBK 44 HDPE pipe
(discontinued **) LACQTENE® 2001 PBK 44 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2001 PBK 44 is a black compound especially developed for s.. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 374 °F |
GB3682 |
JPJ Technologies HDPE Pipe Grade Information provided by JPJ Technologies |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes BEC5012 is a high molecular weight, low flow rate polypropylene block copolymer with very high impact strength. Applications: BEC5012 is recommended for non-pressure pipes and fittings, structured.. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis BL2631 High Density Polyethylene BL2631 is a high density polyethylene homopolymer intended for blow molding of products requiring high toughness and stiffness. Applications: fresh milk bottles, and juice bottles.Information provi.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borcoat™ HE3453 Natural High Density Polyethylene for Steel Pipe Coating Borcoat HE3453 is a natural and colorable high density polyethylene produced with the Borstar technology in similar conditions as the black ready made top coat Borcoat HE3450. Borcoat HE3453 is rec.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 38 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® TB 38 HDPE Made for tape applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin Product Description: Exact 9061 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin Product Description: Exact 9061 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exact™ 9071 Ethylene-based Plastomer Resin Product Description: Exact 9071 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-709 ABS Super impact |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 1501E Description: Extrusion GradeInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 3500 EF-Low Gel Extrusion Grade, Low Gel Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 6501 Injection Molding Grade, Extra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 9500B Description: Blow Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS TM 25 Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA 91802 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S319 Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA TW-15H Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat Resistance, High IzodInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA TW-23V Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Melt Flow | 0.50 g/10 min @Load 2.16 kg |
0.50 g/10 min @Load 4.76 lb |
ASTM D1238/E |
Borealis Borstar® HE6062 HDPE Black Jacketing Compound Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketin.. |
|||
Melt Flow | 0.50 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.50 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
Carmel Olefins CARMELTECH™ QB 79 P Polypropylene Random Copolymer for Pressure Pipe CARMELTECH™ QB 79 P is a high molecular weight, low melt flow rate polypropylene random copolymer, especially designed for extrusion of pressure pipes and injection molding of fittings. This grade .. |