Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lacqtene® 2001 PBK 44 HDPE pipe  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LACQTENE® 2001 PBK 44 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2001 PBK 44 is a black compound especially developed for sewage pipe. LACQTENE® 2001 PBK 44 is best processed between 190 and 230°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ISO 1183
Oxidative Induction Time (OIT) >= 20 min
>= 20 min
200°C; EN 728
Carbon Black Loading 2.25 %
2.25 %
Melt Flow 0.10 g/10 min

@Load 2.16 kg
0.10 g/10 min

@Load 4.76 lb
ISO 1133
0.50 g/10 min

@Load 5.00 kg
0.50 g/10 min

@Load 11.0 lb
ISO 1133
High Load Melt Index 12 g/10 min

@Load 21.6 kg
12 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ISO 868
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527-2
Elongation at Break >= 700 %
>= 700 %
ISO 527-2
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Melting Point 129 °C
264 °F
ISO 3146
Vicat Softening Point 120 °C
248 °F
ISO 306
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.
Users viewing this material also viewed the following: