Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NIZHNEKAMSKNEFTEKHIM PE 4153L (524F6) High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PE 4153L (524F6) High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.950 - 0.954 g/cc
0.0343 - 0.0345 lb/in³
Base Resin; ASTM D1505
Melt Flow 0.50 - 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 - 0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
15 - 35 g/10 min

@Load 21.6 kg,
Temperature 190 °C
15 - 35 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio 30-50; ASTM D1283