Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.0 - 9.0 g/10 min | 5.0 - 9.0 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE D 6606 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 5.0 - 9.0 g/10 min | 5.0 - 9.0 g/10 min | ASTM D1238-95 |
S&E Specialty Polymers GPP™ 1005M-EX10 Natural PP Application: UL94 V-2, Non-blooming flame-retardant polypropylene compound for injection moldingInformation provided by S&E Specialty Polymers |
|||
Melt Flow | 6.0 - 9.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
6.0 - 9.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
NIZHNEKAMSKNEFTEKHIM 825 High Impact Polystyrene Grade 825 is a high impact polystyrene for injection molding. The polymer's ability to be molded on fast cycles with minimal stresses results in outstanding impact retention. It is used in such ap.. |
|||
Melt Flow | 6.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PP 8332M (EPC40R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 4.0 - 9.0 g/10 min @Load 11.6 kg, Temperature 250 °C |
4.0 - 9.0 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Melt Flow | 4.0 - 9.0 g/10 min @Load 11.6 kg, Temperature 250 °C |
4.0 - 9.0 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Melt Flow | 4.0 - 9.0 g/10 min | 4.0 - 9.0 g/10 min | ASTM D1238 |
Polymer Resources PPX-GP1-[color]EN Modified PPO, Extrusion Grade with HDT of 265 F Process: Extrusion Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 4.0 - 9.0 g/10 min @Load 11.6 kg, Temperature 250 °C |
4.0 - 9.0 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
Melt Flow | 1.0 - 9.0 g/10 min @Load 11.6 kg, Temperature 250 °C |
1.0 - 9.0 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica.. |
|||
Melt Flow | 3.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Melt Flow | 4.0 - 9.0 g/10 min | 4.0 - 9.0 g/10 min | ASTM D1238 |
Polymer Resources PPX-GP1 Modified PPO, General Purpose with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 5.0 - 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 - 9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylex® P1010G20 HB Polycarbonate, 20% Fiberglass Reinforced Information provided by Ravago. |
|||
Melt Flow | 4.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 275 °C |
4.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 527 °F |
ASTM D1238 |
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
Melt Flow | 6.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem HD 7555 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 7.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 0952 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 6.0 - 9.0 g/10 min | 6.0 - 9.0 g/10 min | ASTM D1238 |
Micropol Microlin ML53 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Melt Flow | 7.0 - 9.0 g/10 min | 7.0 - 9.0 g/10 min | ASTM D1238 |
Micropol Microlin ML91 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Melt Flow | 7.0 - 9.0 g/10 min | 7.0 - 9.0 g/10 min | ASTM D1238-94 |
Micropol Microstat ML21 Linear medium density static dissipative polyethylene Information provided by Micropol Limited |
|||
Melt Flow | 3.0 - 9.0 g/10 min @Load 5.00 kg, Temperature 250 °C |
3.0 - 9.0 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Kraton® G7723 G Linear Triblock Copolymer Description: Kraton G7723 GS-N is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: G4610 HU - supplied as an und.. |
|||
Melt Flow | 4.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 235 °C |
4.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1100-211XG Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 7.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 0950 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 6.0 - 9.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
6.0 - 9.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Kureha KF Polymer 1000 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Melt Flow | 5.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 177 °C |
5.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 351 °F |
|
Taiwan Sheen Soon Sheenthane® AH-583 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 4.0 - 9.0 g/10 min | 4.0 - 9.0 g/10 min | 190/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® RP-HDPE High Density Polyethylene Polifil® RP-High Density Polyethylene is a moderate stiffness material that retains excellent toughness. HDPE exhibits outstanding chemical resistance and environmental stress crack resistance. Inj.. |
|||
Melt Flow | 5.0 - 9.0 g/10 min | 5.0 - 9.0 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX D6509 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Melt Flow | 5.0 - 9.0 g/10 min | 5.0 - 9.0 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPP 3005 GR BLK Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Melt Flow | 3.0 - 9.0 g/10 min | 3.0 - 9.0 g/10 min | ASTM D1238-92 |
Iran Petrochemical (PCC) Tabriz WT1235 High Impact Polystyrene
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 5.0 - 9.0 g/10 min | 5.0 - 9.0 g/10 min | ASTM D1238 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 5.0 - 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 - 9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylex® P1010G15 HB Polycarbonate, 15% Fiberglass Reinforced Information provided by Ravago. |
|||
Melt Flow | 5.0 - 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.0 - 9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE2NT 11-285D High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure pipes and connection elements for pipeline phase method. Application: Composition is intended to be processed into pressure pipes.. |