Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® RP-HDPE High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® RP-HDPE High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polifil® RP-High Density Polyethylene is a moderate stiffness material that retains excellent toughness. HDPE exhibits outstanding chemical resistance and environmental stress crack resistance. Injection molding applications range from small containers and lids to large crates and bins. Low melt flow versions are used for blow molded bottles for milk, cosmetics, and chemicals, and in extruded items such as pipes and profiles. High molecular weight (HMW) grades are increasingly used for high strength blown films, and large blow molded items such as drums, water tanks, and toys.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Water Absorption 0.00 %
0.00 %
24 hours; ASTM D570
Melt Flow 4.0 - 9.0 g/10 min
4.0 - 9.0 g/10 min
190/2.16; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 65.6 °C
150 °F
ASTM D648
Users viewing this material also viewed the following: