Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 9.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 5.0 - 9.0 g/10 min
5.0 - 9.0 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Flex® TPE D 6606 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Melt Flow 6.0 - 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 - 9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
NIZHNEKAMSKNEFTEKHIM 825 High Impact Polystyrene
Grade 825 is a high impact polystyrene for injection molding. The polymer's ability to be molded on fast cycles with minimal stresses results in outstanding impact retention. It is used in such ap..
Melt Flow 5.0 - 9.0 g/10 min
5.0 - 9.0 g/10 min
ASTM D1238
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 4.0 - 9.0 g/10 min

@Load 11.6 kg,
Temperature 250 °C
4.0 - 9.0 g/10 min

@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Melt Flow 4.0 - 9.0 g/10 min

@Load 11.6 kg,
Temperature 250 °C
4.0 - 9.0 g/10 min

@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade
Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc..
Melt Flow 1.0 - 9.0 g/10 min

@Load 11.6 kg,
Temperature 250 °C
1.0 - 9.0 g/10 min

@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant
Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica..
Melt Flow 3.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
3.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Melt Flow 5.0 - 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 - 9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Ravago Manufacturing Americas Hylex® P1010G10 HB Polycarbonate, 10% Fiberglass Reinforced
Information provided by Ravago.
Melt Flow 5.0 - 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 - 9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Ravago Manufacturing Americas Hylex® P1310G15 HB Polycarbonate, 15% Fiberglass Reinforced, UV Stabilized
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Melt Flow 4.0 - 9.0 g/10 min
4.0 - 9.0 g/10 min
ASTM D1238
Polymer Resources PPX-GP1 Modified PPO, General Purpose with HDT of 265 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 5.0 - 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 - 9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Ravago Manufacturing Americas Hylex® P1010G20 HB Polycarbonate, 20% Fiberglass Reinforced
Information provided by Ravago.
Melt Flow 4.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 275 °C
4.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat..
Melt Flow 5.0 - 9.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
5.0 - 9.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound
BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial..
Melt Flow 6.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem HD 7555 LS-L HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Melt Flow 7.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem PH 0952 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Melt Flow 6.0 - 9.0 g/10 min
6.0 - 9.0 g/10 min
ASTM D1238
Micropol Microlin ML53 Linear Polyethylene Rotational Molding Powder
Information provided by Micropol Limited
Melt Flow 7.0 - 9.0 g/10 min
7.0 - 9.0 g/10 min
ASTM D1238
Micropol Microlin ML91 Linear Polyethylene Rotational Molding Powder
Information provided by Micropol Limited
Melt Flow 7.0 - 9.0 g/10 min
7.0 - 9.0 g/10 min
ASTM D1238-94
Micropol Microstat ML21 Linear medium density static dissipative polyethylene
Information provided by Micropol Limited
Melt Flow 3.0 - 9.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
3.0 - 9.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Kraton® G7723 G Linear Triblock Copolymer
Description: Kraton G7723 GS-N is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: G4610 HU - supplied as an und..
Melt Flow 7.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem PH 0950 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Melt Flow 6.0 - 9.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
6.0 - 9.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Kureha KF Polymer 1000 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Melt Flow 5.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 177 °C
5.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 351 °F
Taiwan Sheen Soon Sheenthane® AH-583 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Melt Flow 6.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 275 °C
6.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
Solvay Specialty Polymers Halar® 6012F Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Halar® 6012F is semi-crystalline fluoropolymer designed specifically for rotational molding and lining. Rotomolding is typically used to manufacture articles such as tanks, bottles and vessels wh..
Melt Flow 5.0 - 9.0 g/10 min
5.0 - 9.0 g/10 min
ASTM D1238
Buckeye Polymers BP FLEX D6509 CU BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
Melt Flow 5.0 - 9.0 g/10 min
5.0 - 9.0 g/10 min
ASTM D1238
Buckeye Polymers BP RPP 3005 GR BLK Polypropylene, Glass Filled
Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en..
Melt Flow 3.0 - 9.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
3.0 - 9.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers.
Melt Flow 3.0 - 9.0 g/10 min
3.0 - 9.0 g/10 min
ASTM D1238-92
Iran Petrochemical (PCC) Tabriz WT1235 High Impact Polystyrene  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Melt Flow 5.0 - 9.0 g/10 min
5.0 - 9.0 g/10 min
ASTM D1238
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 5.0 - 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 - 9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Ravago Manufacturing Americas Hylex® P1010G15 HB Polycarbonate, 15% Fiberglass Reinforced
Information provided by Ravago.
Melt Flow 5.0 - 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 - 9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
±10%
Kazanorgsintez PE2NT 11-285 High Density Polyethylene Composite
Production Method: Copolymerization of eythylene at low pressure pipes and connection elements for pipeline phase method. Application: Composition is intended to be processed into pressure pipes..
Copyright © lookpolymers.com All Rights Reserved