Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
ASTM D792
Melt Flow 7.0 - 9.0 g/10 min
7.0 - 9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
50mm/min; ASTM D638-64T
Elongation at Break 300 %
300 %
ASTM D638-64T
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D760-66
Impact 19

@Temperature -20.0 °C
19

@Temperature -4.00 °F
J/mm, Falling weight impact; ARM
Thermal Properties Metric English Comments
Vicat Softening Point 108 °C
226 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Flammability, UL94 V-2
V-2
Oxygen Index 26 %
26 %
Critical
Descriptive Properties Value Comments
British Standard 2782:508A Zero Burn Rate
British Standard 476 Part 7 Class 2
Civil Aviation Authority Spec No 8 Vertical Test Pass