Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ASTM D955 |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 3.17 mm |
0.016 - 0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 7210 Black Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm @Thickness 3.17 mm |
0.012 - 0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000MDL Nylon 6/6
(discontinued **) Available in North America Additive: Molybdenum Disulfide Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedForm: Pellets Information provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm @Thickness 3.20 mm |
0.014 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP1007F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
LATI Later 4-V0HF1 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm @Thickness 3.20 mm |
0.015 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Linear Mold Shrinkage, Flow | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP IB008 PA 6/12 (Europe-Africa-Middle East) LNP* Thermocomp* IB008 is a compound based on Nylon 6/12 resin containing Glass Bead. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT 4.2 specific gravity, PBT, gray |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm | 0.016 - 0.018 in/in | annealed 130C 1hr; ASTM D955 |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific) Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX963 PPE+PA (Europe-Africa-Middle East) NORYL GTX963 is an unfilled impact modified material with excellent heat properties and good processability. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX964 PPE+PA (Europe-Africa-Middle East) NORYL GTX964 is an unfilled impact modified material with optimised processability. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX976 PPE+PA (Europe-Africa-Middle East) NORYL GTX976 is a material especially designed for electrostatic painting and powder coating applications. This material combines high impact performance with conductivity in an unique way.This data.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm @Thickness 3.20 mm |
0.015 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled productThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm @Thickness 3.20 mm |
0.015 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-LOY SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled product |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm | 0.012 - 0.018 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.018 cm/cm @Thickness 4.00 mm |
0.012 - 0.018 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA66 D91 PA66, Aramid Fiber Filled, Injection Molded Star L PA66 D91 is a PTFE lubricated, Aramid Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm | 0.016 - 0.018 in/in | on Tensile Bar; E2P method |
Eurostar Staramide Z1000XXC PA66, Injection Molded Staramide Z1000XXC is an UV Stabilized Polyamide 66 Injection Molding Resin (also known as R1000HI0944)Information provided by Eurostar. |