Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycolac® GRM2600L ABS High Impact , good chemical resistance sheet grade ABS designed for refrigerator liner applications. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9130T PC COPOLYMER (Asia Pacific) LUX9130T Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm / 5VA rating at 6.0mm and is U.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0060 cm/cm | 0.0045 - 0.0060 in/in | |
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0070 cm/cm | 0.0045 - 0.0070 in/in | |
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0070 cm/cm | 0.0045 - 0.0070 in/in | |
LATI Latan 13 G/30 POM, 30% Glass Fiber Reinforced Polyoxymethylene (POM) based compound. Glass fibers. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0080 cm/cm | 0.0045 - 0.0080 in/in | |
LATI Laticonther 52/11 GR/70 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0060 cm/cm | 0.0045 - 0.0060 in/in | |
LATI Laticonther 75 CPG/650 PBT, Glass Fiber Reinforced High thermal conductivity product based on Polybutylene Terephthalate (PBT). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0070 cm/cm | 0.0045 - 0.0070 in/in | |
LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced High thermal conductivity product based on Polycarbonate (PC). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0075 cm/cm | 0.0045 - 0.0075 in/in | |
LATI Latilub 80-10T Y/15 PPS, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0075 cm/cm | 0.0045 - 0.0075 in/in | |
LATI Latilub 80-40GRT PPS, Graphite/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Graphite / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO 294-4 |
Solvay Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This p.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO Data |
Styrolution Luran® S 757 G ASA Luran S 757 G is an easy flowing injection molding ASA grade with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO Data |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO Data |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0055 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0055 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific) Modified PPO Resin with 20% Glass Fibre Reinforced |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | ISO DIS 294-4 |
Wellman Wellamid® WE1408 13% Glass Fiber Reinforced Engineering Grade Nylon 66 Description: Glass Fiber Reinforced Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0065 cm/cm @Thickness 3.00 mm |
0.0045 - 0.0065 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® FR3009 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | Sim. To ISO 294-4 |
DSM Arnite® AV2 390 XT PET GF50 50% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Luranyl® KR 2454/3 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced Heat resistant grade with halogen-free flame retardant; applications include TV plug connectors and components in switchgear cabinets.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Polystyrol® 165 H Polystyrene (Europe) High molecular grades, often blended with high-impact extrusion grades (e.g. for dairy products).Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Polystyrol® 168 N Polystyrene (Europe) High molecular, heat-resistant grades used where high strength is required. Suitable for expanded film.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Polystyrol® 168 NO Polystyrene (Europe) High molecular, heat-resistant grades for the extrusion of low-taint food packaging, especially BOPS.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | TM=300°C, TW=80°C |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | TM=300°C, TW=80°C |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO 2577 |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Luranyl® KR 2403 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced General-purpose grade with 10% glass fiber for parts requiring especially good resistance to heat deformation.Applications: auto parts, steering-column cladding and water meters.Data was collected b.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | |
BASF Polystyrol® 143 EO Polystyrene (Europe) Easy flowing grade for the injection molding and extrusion of low-taint food packaging.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0085 cm/cm | 0.0045 - 0.0085 in/in | on Tensile Bar; ISO 294 |
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | ISO 2577 |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors.. |