| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0085 cm/cm | 0.0060 - 0.0085 in/in | ASTM D955 |
| Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0085 cm/cm | 0.0060 - 0.0085 in/in | ASTM D955 |
| Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
| Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm | 0.0065 - 0.0085 in/in | |
| LATI Latamid 12 CP/85 PA 12 Polyamide 12 (PA12) based compound. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
| Linear Mold Shrinkage, Flow | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
| LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;.. |
|||
| Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm | 0.0065 - 0.0085 in/in | |
| LATI Laticonther 83 CP/80 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
| Linear Mold Shrinkage, Flow | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
| LATI Latimass 82-03 D080 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0085 cm/cm | 0.0060 - 0.0085 in/in | |
| LATI Latishield 36/AR-10A-V0E ABS, Steel Fiber Reinforced, Flame Retardant EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Information provided by Lati Indust.. |
|||
| Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm | 0.0065 - 0.0085 in/in | |
| LATI Latishield 36/SP-05A ABS, Steel Fiber Reinforced EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |
|||
| Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm | 0.0065 - 0.0085 in/in | on Tensile Bar; SABIC Method |
| SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0085 cm/cm | 0.0060 - 0.0085 in/in | |
| Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI) Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic.. |
|||
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0085 cm/cm | 0.0060 - 0.0085 in/in | |
| Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI) Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA.. |
|||
| Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm @Thickness 3.00 mm |
0.0065 - 0.0085 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
| Covestro Bayblend® T65 AT PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
| Linear Mold Shrinkage, Flow | 0.0065 - 0.0085 cm/cm @Thickness 3.00 mm |
0.0065 - 0.0085 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
| Covestro Bayblend® T65 HI PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature .. |
|||
| Linear Mold Shrinkage, Flow | 0.0045 - 0.0085 cm/cm | 0.0045 - 0.0085 in/in | on Tensile Bar; ISO 294 |
| Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
| Linear Mold Shrinkage, Flow | 0.0045 - 0.0085 cm/cm | 0.0045 - 0.0085 in/in | on Tensile Bar; ISO 294 |
| Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0085 cm/cm | 0.0060 - 0.0085 in/in | ASTM D955 |
| Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |
|||
| Linear Mold Shrinkage, Flow | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
| LATI Latimass 82-03 D110 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||