Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | ISO 294-4 |
Polyplastic Armamid® PA GF25-1FR Nylon 6, 25% Glass Fiber Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | Injection molding; ISO 2577 |
Hexion Bakelite™ PF 6507 Phenolic Formaldehyde Resin, Elasticized, Low Shrinkage, Resistant to High Temperatures, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, hi.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | |
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
LATI Latilub 87/28-15T K/20 PC, 20% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem 3451 PEI 45% Glass fiber and mineral filled, standard flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS CF15 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | |
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® HIPS GF30 30% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA4/6 CF40 HS 40% Carbon Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+PS LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-KON WEF32ISP PBT (Europe-Africa-Middle East) LNP * Stat-kon* WEF32ISP is a compound based on Polybutylene Terephalate resin containing Glass Fiber and Carbon Fiber. Added features include High Impact, Heat Stabilized and Electrically Conduct.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PES GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 9822121Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS GF20 LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | GB/T 15585-1995 |
Sichuan Deyang Haton® hMR61 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Time 86400 sec |
0.0015 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RV00AESC PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESC is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | 48h at 80°C; ISO 294-4 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0035 cm/cm @Thickness 4.00 mm |
0.0015 - 0.0035 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide PF00AS PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00AS is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | ISO 294-4 |
Barlog Plastics KEBAFLOW MX130 LCP, 30% glass fiber / mineral reinforced LCP-GF/MD 30Information provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | ISO 294 |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | |
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS CF40 BK 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |