Material Notes:
LCP-GF/MD 30Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0603 lb/in³
ISO 1183
Water Absorption 0.030 %
0.030 %
similar to ISO 62 test
Linear Mold Shrinkage, Flow 0.0015 cm/cm
0.0015 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0042 cm/cm
0.0042 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
ISO 527-1
Elongation at Break 2.3 %
2.3 %
ISO 527-1
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 268 °C
514 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL Registered; IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Descriptive Properties Value Comments
Resin Type LCP-GF/MD 30