Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D955 |
PTS PPE-LXS 314-30 PPE-HIPS, 30% Glass Filled Typical Applications: Water industrial partsInformation provided by PTS LLC. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Fittings 210(HR) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Fittings 210A Gray 172(HS) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Fittings 87322 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 2.00 mm |
0.0030 - 0.0050 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® CE15315 BK010 PBT
(Unverified Data**) Crastin® CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID SG2600B PA6+GF60%, General purpose, Good Surface Feature: Injection Molding, PA6+GF60%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0050 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOY SC3154 PC+GF15% Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Thickness 3.17 mm |
0.0020 - 0.0050 in/in @Thickness 0.125 in |
ASTM D955 |
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | |
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Time 86400 sec |
0.0020 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66 LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM HU2210 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® SHF436HR PBT PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DX05475 PC LNP* THERMOCOMP* DX05474 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ISO 294-4; ASTM D955 |
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp RF007S PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF007S is a compound based on PA 66 resin containing Glass Fiber . Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp RFB53SUZ PA 66 LNP THERMOCOMP* RFB53SUZ is a compound based on Nylon 66 resin containing Glass Bead, Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for th.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Time 86400 sec |
0.0020 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF1750-N2 50% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRGF25/15 42H-NBK1 40% Mineral/Glass Fiber Reinforced Nylon 6 Description: Mineral/Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | |
Eastman Eastar 6763 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
ASTM D955 |
Eastman Eastar DN114 Copolyester, Natural Applications:LightingProduct Description: Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage. DN1.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 4.00 mm |
0.0030 - 0.0050 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starflam RX06082 PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Staramide RX06082 is a Halogen Free and Red Phosphorous Free, flame Retardant, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |