Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | ASTM D955 |
PolyOne OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0015 cm/cm | 0.0010 - 0.0015 in/in | ASTM D955 |
PolyOne Edgetek® PC-15CF-15GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0015 cm/cm | 0.0010 - 0.0015 in/in | ASTM D955 |
PolyOne Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0015 cm/cm @Thickness 3.18 mm |
0.0010 - 0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® X TR2-20GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | Solvay Test |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | |
LATI Latilon 28D K/40 PC, 40% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data .. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP UCL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36ASP is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0015 cm/cm | 0.00 - 0.0015 in/in | |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Time 86400 sec |
0.00050 - 0.0015 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX13320C PC COPOLYMER (Asia Pacific) LNP* Statkon DX13320C is ultra clean polycarbonate/carbon fiber compound with high modulus, good flow ability, easy mold release, and high level of cleanliness for the most demanding application. A .. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Time 86400 sec |
0.00050 - 0.0015 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00060 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC LNP* Stat-kon* Lexan_LC1500N compound is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East) LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1010 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* HMC1010 compound is a 10% Carbon fiber reinforced. Static dissipative. Nonbrominated, nonchlornated flame retardant system. UL94 V-1 rated. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+PS LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific) DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
Linear Mold Shrinkage, Flow | 0.00090 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00090 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Linear Mold Shrinkage, Flow | 0.00090 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00090 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Linear Mold Shrinkage, Flow | 0.00090 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00090 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON DX09303C PC (Asia Pacific) LNP* Stat-Kon* DX09303C is carbon fiber filled polycarbonate composite with high modulus, good flow ability, and high level of cleanliness for the most demanding application. A unique feature of thi.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP RC00A PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC00A is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0015 cm/cm | 0.0010 - 0.0015 in/in | on Tensile Bar; E2P method |
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0015 cm/cm | 0.00 - 0.0015 in/in | ASTM D955 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |
|||
Linear Mold Shrinkage, Flow | 0.00030 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00030 - 0.0015 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUXY KS G55 Amorphous PA6 Description: Injection Molding, Amorphous PA6, High Modulus, High Impact, Low WarpageApplication: Electric/Electronic Components (LCD Bracket)Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | Solvay Test |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Linear Mold Shrinkage, Flow | 0.00090 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00090 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |