PolyOne Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU)

Category Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0015 cm/cm
0.0010 - 0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 121 MPa
17500 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 190 MPa
27600 psi
ASTM D790
Flexural Modulus 6.89 GPa
999 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 213 °C

@Thickness 3.18 mm
415 °F

@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 V-0
V-0
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+6 ohm
1.00e+6 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 360 - 393 °C
680 - 739 °F
Mold Temperature 121 - 163 °C
250 - 325 °F
Drying Temperature 149 °C
300 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Filler / Reinforcement GlassCarbon Fiber Reinforcement
Forms Pellets
Generic Material PPSU
Generic Name Polyphenylsulfone (PPSU)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America