Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyamide-imide (PAI)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal expansion characteristics similar to steel, and therefore excellent dimensional stability. Torlon PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep, and chemicals. The potential applications for this resin include metal replacement, sliding vanes, aerospace parts, impellors, shrouds, pistons, and housings. It is available in injection molding and extrusion (E) grades.Injection Notes: Minimum drying conditions: 3 hours at 350°F (177°C), 4 hours at 300°F (149°C), or 16 hours at 250°F (121°C). Compression Ratio: 1:1 to 1.5:1 Begin hold pressure at a high setting 6,000-8,000 psi (41.37-55.16 MPa), for several seconds, then drop off to 3,000-5,000 psi (20.69-34.48 MPa), for the duration of the hold pressure sequence. Molded parts must be post cured.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Filler Content 30 %
30 %
Carbon Fiber Reinforcement
Water Absorption 0.26 %

@Time 86400 sec
0.26 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.00 - 0.0015 cm/cm
0.00 - 0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 221 MPa
32100 psi
ASTM D638
Tensile Stress 203 MPa
29400 psi
ASTM D1708
Elongation at Break 1.5 %
1.5 %
ASTM D638
6.0 %
6.0 %
ASTM D1708
Tensile Modulus 16.5 GPa
2390 ksi
ASTM D638
22.3 GPa
3230 ksi
ASTM D1708
Flexural Strength 174 MPa

@Temperature 232 °C
25200 psi

@Temperature 450 °F
ASTM D790
350 MPa

@Temperature 23.0 °C
50800 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 15.7 GPa

@Temperature 232 °C
2280 ksi

@Temperature 450 °F
ASTM D790
19.9 GPa

@Temperature 23.0 °C
2890 ksi

@Temperature 73.4 °F
ASTM D790
Compressive Strength 254 MPa
36800 psi
ASTM D695
Compressive Modulus 9.86 GPa
1430 ksi
ASTM D695
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
3.20 J/cm
5.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C
5.00 µin/in-°F
ASTM D696
Thermal Conductivity 0.520 W/m-K
3.61 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 282 °C
540 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 304 °C
579 °F
Nozzle Temperature 371 °C
700 °F
Mold Temperature 199 - 216 °C
390 - 421 °F
Drying Temperature 177 °C
351 °F
Dry Time 3.00 hour
3.00 hour
Moisture Content 0.050 %
0.050 %
Back Pressure 6.89 MPa
999 psi
Screw Speed 50 - 100 rpm
50 - 100 rpm
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Fatigue Resistant
Flame Retardant
Good Chemical Resistance
Good Compressive Strength
Good Creep Resistance
Good Dimensional Stability
High Heat Resistance
High Stiffness
High Temperature Strength
Semi Conductive
Forms Pellets
Generic PAI
Processing Method Injection Molding
Machining
Profile Extrusion
RoHS Compliance RoHS Compliant
Screw L/D Ratio 18.0:1.0 to 24.0:1.0
Uses Aerospace Applications
Aircraft Applications
Business Equipment
Connectors
Electrical/Electronic Applications
Film
Gears
Housings
Industrial Applications
Industrial Parts
Machine/Mechanical Parts
Metal Replacement
Oil/Gas Applications
Semiconductor Molding Compounds
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved