Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® RCM6134 PC+ABS (Asia Pacific) Cycoloy* RCM6134 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1... |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4 |
DSM Akulon® K-FHG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
LATI Latilub 66-01M G/50 PA66, 50% Glass Fiber Reinforced, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | |
LATI Latiohm 80-05 CNT GCE/500 PPS, Glass/Mineral Reinforced Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Carbon nanotubes. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PA6 GF33 FR HS L BK065 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/10 GF50 L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Time 86400 sec |
0.0030 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON SE002Z PA 12 (Asia Pacific) LNP* Stat-kon* SE002Z is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PC GF30 TS15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Com.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Time 86400 sec |
0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP JF004P PES (Asia Pacific) LNP* Thermocomp* JF004P is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Exceptional Processing. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0040 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0040 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® TF-0930 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 (Asia Pacific) LNP THERMOCOMP* RF0049S is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP fo.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® HDPE LGF50 12 mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | MD |
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced Applications: HousingsBracketsGear casesFeatures: High RigidityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Thickness 4.00 mm |
0.0030 - 0.0050 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starglas FF006 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | Eurotec |
Eurotec® Tecomid® NB30 GR15 BK005 FS90 PA6, 15% glass fiber reinforced, flame retardant - halogen & red phosphorus free, low smoke & toxic gas grade Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | Eurotec |
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | Eurotec |
Eurotec® Tecomid® NB40 GR20 NL XA70 PA6, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4 |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ASTM and ISO value |
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron GR630 HS is a heat stabilized, 30% glass fiber reinforced polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This ba.. |