Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ASTM D955 |
PolyOne LubriOne™ NI-0920063 NATURAL Polyamide 610 (Nylon 610) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose Feature: Injection Molding, SAN+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2410R PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Time 86400 sec |
0.0010 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP D351 PC (Asia Pacific) LNP* Thermocomp* D351 (experimental grade name as EXTC8143) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus,.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm @Time 86400 sec |
0.0010 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Time 86400 sec |
0.0010 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON EV008 PEI LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL NC220 PPE+HIPS (Asia Pacific) |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm @Time 86400 sec |
0.0010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RE006 PA6.6 (Asia Pacific) LNP STAT-KON RE006 is a compound based on Nylon 66 containing carbon fiber. Added features of this material include: Electrically Conductive. Also known as STAT-KON RC-1006 |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Chase Plastics CP Pryme® PC320R Polycarbonate, Recycled Content Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65 Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSGL-40/4 FA black 9840 PA666-GF40 Product description: Grilon TSGL-40/4 FA black 9840 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 FA black 9840 is characterized by th.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA) 55% Glass Reinforced PPA High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Linear Mold Shrinkage, Flow | <= 0.0010 cm/cm | <= 0.0010 in/in | ISO 294-4 |
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4 |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ISO 294-4 |
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled Injection molding, heat stabilizedInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | Compression molding; ISO 2577 |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |