Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955-89 |
Multibase Multi-Flex® TPO DEFA 1047 The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955-89 |
Multibase Multi-Pro® 2518 CU 25% Mineral Filled Polypropylene Multi-Pro 2518 CU is a mineral reinforced polypropylene compound offering overall balanced impact and stiffness properties. This material is specially formulated with UV stabilization for outdoor ex.. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Multibase Multi-Pro® 4518 CUW Polypropylene Calcium Carbonate Filler, 45% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH TS15040 D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 KV25 Nylon 6 for injection molding, 25% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm | 0.0090 - 0.014 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYform POM C M90 GF10 Polyoxymethylene Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ F40 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | (longitudinal) Injection; ISO 2257 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | FRISETTA Test Method |
Nilit RECONYL A KV30 Recycled nylon 6.6 for injection molding, 30% glass ball reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | |
Lehmann & Voss LUVOCOM® 1105-8174 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.015 cm/cm | 0.0090 - 0.015 in/in | |
Lehmann & Voss LUVOCOM® 1105-8292 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D995 |
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially.. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Multibase Multi-Flex® D 5308 Platinum TPO Thermoplastic Polyolefin Elastomer Forms: PelletsInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | Injection molded; ASTM D955 |
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN .. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
Lubrizol Estane® S190A Thermoplastic Polyurethane Type: Estane® S190A is a Shore 92A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ASTM D955 |
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has .. |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | disk |
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.013 cm/cm | 0.0090 - 0.013 in/in | Flow direction; ASTM D955 |
Lubrizol Estane® 2355-55DE Thermoplastic Polyurethane Type: Pellethane® 2355-55DE is a thermoplastic polyurethane elastomer.Information Provided by The Lubrizol Corporation |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0334M20CL Mica Reinforced Coupled |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0334T30L1 Talc Reinforced |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0334W20L1 Wollastonite Reinforced |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0336M10CL Mica Reinforced Coupled |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm @Thickness 4.00 mm |
0.0090 - 0.011 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ISO data |
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions.. |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0090 - 0.014 in/in @Thickness 0.126 in, Time 72.0 hour |
ASTM D955 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |