Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D-955 |
Plaskolite Optix® CA - 51 FDA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D-955 |
Plaskolite Optix® CA - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D-955 |
Plaskolite West Optix® CP - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | With Flow; ISO 2577 |
Polykemi AB SCANTEC PC S60R GF10 Polycarbonate, Glass-Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 3.17 mm |
0.0020 - 0.0050 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylex® P1010G7FRMA Polycarbonate, 7% Glass Filled Polycarbonate, 7% Glass Filled, Flame RetardantInformation provided by Ravago. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ISO 2577 |
NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 7% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 17% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955-51 |
Lucky EG-930 Acrylic, Injection Grade Injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | |
Lehmann & Voss LUVOCOM® 1-7943 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 3.17 mm |
0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plaslube® J-1/30/TF/10 Nylon 66, 30% GFR, 10% PTFE Plaslube glass fiber reinforced, polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer an excellent balance of wear and friction performance and mechanical strength. The addition of silic.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.012 cm/cm | 0.0020 - 0.012 in/in | ASTM D955 |
Samyang Tribit® 1550GN30 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN30 is a reinforced, flame retardant (.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
PlastxWorld CEVIAN® B5536 30% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ISO 294-4 |
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 3.175 mm |
0.0020 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
Eastman Eastar DN004HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN004HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | |
E-Polymers TEKASTER® F615G55 55% Glass Fiber Reinforced High Modulus PET Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | ASTM D955 |
A. Schulman ComAlloy Hiloy® 213 Polystyrene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | ASTM D955 |
A. Schulman ComAlloy Voloy® 461 Glass Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | ASTM D2566-69 |
BCC Products BC 7062-2H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical .. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | ASTM D955 |
LNP Thermocomp® JF-1006 E LE BK8-055 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Features: High Viscosity, Low ExtractablesForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | ASTM D955 |
Aaron Industries AAROPRENE® GFIPP 2030 High Impact Glass Filled Polypropylene AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 35% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |