| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled |
| Manufacturer | Polykemi AB |
| Trade Name | SCANTEC |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB SCANTEC PC S60R GF10 Polycarbonate, Glass-Fiber Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.24 g/cc | 0.0448 lb/in³ | ISO 1183 |
| Filler Content | 10 % | 10 % | ±2%; Polykemi |
| Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | With Flow; ISO 2577 |
| 0.0060 cm/cm | 0.0060 in/in | Across Flow; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 45.0 MPa | <= 6530 psi | ISO/R527 |
| Elongation at Break | 7.0 % | 7.0 % | ISO/R527 |
| Flexural Strength | <= 115 MPa | <= 16700 psi | ISO 178 |
| Flexural Modulus | 3.50 GPa <br>@Temperature 23.0 °C |
508 ksi <br>@Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.700 J/cm² <br>@Temperature -20.0 °C |
3.33 ft-lb/in² <br>@Temperature -4.00 °F |
ISO 179 |
| 1.00 J/cm² <br>@Temperature 23.0 °C |
4.76 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 145 °C | 293 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 135 °C | 275 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 145 °C <br>@Load 5.001 kg |
293 °F <br>@Load 11.03 lb |
50°C/h; ISO 306 |
| Flammability, UL94 | V-2 <br>@Thickness 1.60 mm |
V-2 <br>@Thickness 0.0630 in |
|
| V-1 <br>@Thickness 3.20 mm |
V-1 <br>@Thickness 0.126 in |
||
| Glow Wire Test | 960 °C <br>@Thickness 3.20 mm |
1760 °F <br>@Thickness 0.126 in |
IEC 695-2-1 |