Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.51 - 1.70 g/cc | 0.0546 - 0.0614 lb/in³ | Average value: 1.60 g/cc Grade Count:5 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Density | 1.46 - 1.70 g/cc | 0.0527 - 0.0614 lb/in³ | Average value: 1.54 g/cc Grade Count:27 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Density | 1.34 - 1.70 g/cc | 0.0484 - 0.0614 lb/in³ | Average value: 1.41 g/cc Grade Count:21 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Density | 1.29 - 1.70 g/cc | 0.0466 - 0.0614 lb/in³ | Average value: 1.53 g/cc Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Density | 1.09 - 1.70 g/cc | 0.0394 - 0.0614 lb/in³ | Average value: 1.23 g/cc Grade Count:215 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Density | 1.12 - 1.70 g/cc | 0.0405 - 0.0614 lb/in³ | Average value: 1.35 g/cc Grade Count:146 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.41 - 1.70 g/cc | 0.0509 - 0.0614 lb/in³ | Average value: 1.53 g/cc Grade Count:25 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Density | 1.50 - 1.70 g/cc | 0.0542 - 0.0614 lb/in³ | |
Zircar Refractory Composites RS-A Refractory Sheet ZRCI`s Refractory Sheet Type RS-A Moldable is a tough ceramic fiber reinforced insulation which contains no asbestos. Developed as an asbestos board replacement for induction coil liners and molten .. |
|||
Density | 1.60 - 1.70 g/cc | 0.0578 - 0.0614 lb/in³ | ISO 1183 |
BASF Ultradur® B 4406 G3 Uncolored Q717 PBT Information provided by BASF |
|||
Density | 1.60 - 1.70 g/cc | 0.0578 - 0.0614 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Density | 1.60 - 1.70 g/cc | 0.0578 - 0.0614 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |
|||
Density | 1.60 - 1.70 g/cc | 0.0578 - 0.0614 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color.. |
|||
Density | 1.04 - 1.70 g/cc | 0.0376 - 0.0614 lb/in³ | Average value: 1.27 g/cc Grade Count:267 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Density | 1.39 - 1.70 g/cc | 0.0502 - 0.0614 lb/in³ | Average value: 1.50 g/cc Grade Count:19 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Density | 1.46 - 1.70 g/cc | 0.0527 - 0.0614 lb/in³ | Average value: 1.60 g/cc Grade Count:22 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Density | 1.07 - 1.70 g/cc | 0.0387 - 0.0614 lb/in³ | Average value: 1.24 g/cc Grade Count:20 |
Overview of materials for Chlorosulfonated Polyethylene Rubber This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val.. |