Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.41 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
STN EN ISO 1183-1
Plastcom SLOVAMID® 6 GF 40 HI PA6 reinforced with glass fiber, improved impact strength
PA 6 for injection molding, reinforced with 40% glass fiber, impact modified. Application: impacted moldings and moldings with higher strength applied in automotive, electrical, engineering and cons..
Density 1.41 - 1.45 g/cc
0.0509 - 0.0524 lb/in³
ISO R 1184
Fainplast Compounds RI 54 Rigid PVC, Injection Molding
Fittings for building trade - high fluidity
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Density 1.41 g/cc
0.0509 lb/in³
LATI Lapex R G/20 PPSU, 20% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA
LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant.
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p..
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP LX97024 PEEK (Europe-Africa-Middle East)
LNP* LUBRICOMP* LX97024 is a compound based on Polyetheretherketone containing Glass Fiber, PTFE. Added features include: Internally Lubricated, Easy Molding.
Density 1.41 g/cc
0.0509 lb/in³
ASTM D-792
Sumitomo Bakelite North America FM 3001 Cellulose Reinforced Phenolic Novolac
FM 3001 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America...
Density 1.41 g/cc
0.0509 lb/in³
DIN 53479
Polyram RamSter RF350M3 PBT, 15% Mineral Filled
15% mineral filled PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.41 g/cc
0.0509 lb/in³
DIN 53479
Polyram RamTal RM7009 Acetal, UV Stabilized
UV stabilized acetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.41 g/cc
0.0509 lb/in³
(DAM); ISO 1183
DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
EMS-Grivory Grivory® BG-35 S PA6-GF35
Information provided by EMS Grivory
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® 500SC NC010 Acetal (POM)  (Unverified Data**)
Silicone Lubricated Medium Viscosity Acetal Homopolymer Concentrate Developed for Enhancing LubricityInformation provided by DuPont Performance Polymers
Density 1.41 g/cc
0.0509 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® 70G35HSL NC010 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL NC010 is a 35% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM)
Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used ..
Density 1.41 g/cc
0.0509 lb/in³
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid..
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Ashley Polymers Ashlene® RH190TB Acetal
Impact modified reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity, black.Data provided by the manufacturer
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Chem Polymer Formax 604 Acetal, Low Flow
A 4 melt flow index copolymer acetal for extrusion or thick injection molding applications.Data provided by the manufacturer, Chem Polymer.
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
BASF Ultraform S 1320 0021 UNC POM
Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels,..
Density 1.41 g/cc
0.0509 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex..
Density 1.41 g/cc
0.0509 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp QF008S PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF008S is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Copyright © lookpolymers.com All Rights Reserved