Physical Properties Metric English Comments
Density 1.51 - 1.70 g/cc
0.0546 - 0.0614 lb/in³
Average value: 1.60 g/cc Grade Count:5
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
Density 1.46 - 1.70 g/cc
0.0527 - 0.0614 lb/in³
Average value: 1.54 g/cc Grade Count:27
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Density 1.34 - 1.70 g/cc
0.0484 - 0.0614 lb/in³
Average value: 1.41 g/cc Grade Count:21
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum ..
Density 1.29 - 1.70 g/cc
0.0466 - 0.0614 lb/in³
Average value: 1.53 g/cc Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Density 1.09 - 1.70 g/cc
0.0394 - 0.0614 lb/in³
Average value: 1.23 g/cc Grade Count:215
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Density 1.12 - 1.70 g/cc
0.0405 - 0.0614 lb/in³
Average value: 1.35 g/cc Grade Count:146
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Density 1.41 - 1.70 g/cc
0.0509 - 0.0614 lb/in³
Average value: 1.53 g/cc Grade Count:25
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Density 1.50 - 1.70 g/cc
0.0542 - 0.0614 lb/in³
Zircar Refractory Composites RS-A Refractory Sheet
ZRCI`s Refractory Sheet Type RS-A Moldable is a tough ceramic fiber reinforced insulation which contains no asbestos. Developed as an asbestos board replacement for induction coil liners and molten ..
Density 1.60 - 1.70 g/cc
0.0578 - 0.0614 lb/in³
ISO 1183
BASF Ultradur® B 4406 G3 Uncolored Q717 PBT
Information provided by BASF
Density 1.60 - 1.70 g/cc
0.0578 - 0.0614 lb/in³
Molding; IS 867-1963
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded
Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f..
Density 1.60 - 1.70 g/cc
0.0578 - 0.0614 lb/in³
ISO 1138
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound
UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati..
Density 1.60 - 1.70 g/cc
0.0578 - 0.0614 lb/in³
Molding; IS 867-1963
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color..
Density 1.04 - 1.70 g/cc
0.0376 - 0.0614 lb/in³
Average value: 1.27 g/cc Grade Count:267
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Density 1.39 - 1.70 g/cc
0.0502 - 0.0614 lb/in³
Average value: 1.50 g/cc Grade Count:19
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Density 1.46 - 1.70 g/cc
0.0527 - 0.0614 lb/in³
Average value: 1.60 g/cc Grade Count:22
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Density 1.07 - 1.70 g/cc
0.0387 - 0.0614 lb/in³
Average value: 1.24 g/cc Grade Count:20
Overview of materials for Chlorosulfonated Polyethylene Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val..