Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 KG20 Nylon 6.6 for injection molding, 20% chalk filled Nylon 6.6 for injection molding (low warpage and good form stability).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 27% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Density | 1.28 - 1.75 g/cc | 0.0462 - 0.0632 lb/in³ | Average value: 1.43 g/cc Grade Count:232 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | |
LATI Latamid 66 MDT03-01 PA 66 Polyamide 66 (PA66) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | |
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | |
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | |
LATI Latilub 57-10T Y/15 PPA, Aramid Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Conditioned) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem DT1810EV PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.This data was supplied by SABIC-IP for.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU1004 PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
Techmer ES HiFill® ABS E GM30 LE 30% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
Techmer ES HiFill® ABS GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 1018121Information provided by TP Composites, Inc. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
Stir SpA C 2008 AT (PVC) Application: Molding for solesInformation provided by STIR SpA |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PC TL15 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
Teijin Panlite® G-3310M Isotropic, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 10 % of special GF and least anisotropy grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPrecisio.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
Toyobo PELPRENE™ PE450B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
Toyobo PELPRENE™ S2004FS Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® AS LF 20 PA66-Z20 Product description: Grilon AS LF 20 is a heat stabilized, normal viscosity PA 66 injection molding grade with 20% lubricant (PTFE + silicon oil). Grilon AS LF 20 has the following important propert.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon CP-475R Bulk Compound Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arl.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |