Overview of materials for Nylon 6, 40% Glass Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Overview of materials for Nylon 6, 40% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.28 - 1.75 g/cc
0.0462 - 0.0632 lb/in³
Average value: 1.43 g/cc Grade Count:232
1.24 - 1.24 g/cc
<br>@Temperature >=250 °C
0.0448 - 0.0448 lb/in³
<br>@Temperature >=482 °F
Average value: 1.24 g/cc Grade Count:1
Filler Content 35.0 - 45.0 %
35.0 - 45.0 %
Average value: 39.3 % Grade Count:50
Water Absorption 0.200 - 7.10 %
0.200 - 7.10 %
Average value: 3.21 % Grade Count:116
1.50 - 2.10 %
<br>@Temperature 70.0 - 70.0 °C
1.50 - 2.10 %
<br>@Temperature 158 - 158 °F
Average value: 1.80 % Grade Count:4
Moisture Absorption at Equilibrium 0.250 - 6.20 %
0.250 - 6.20 %
Average value: 1.93 % Grade Count:74
Water Absorption at Saturation 4.80 - 7.50 %
4.80 - 7.50 %
Average value: 5.92 % Grade Count:34
Additive Loading 40.0 %
40.0 %
Average value: 40.0 % Grade Count:3
Viscosity 2.60 - 50.0 cP
2.60 - 50.0 cP
Average value: 18.4 cP Grade Count:3
190000 - 190000 cP
<br>@Temperature 280 - 280 °C
190000 - 190000 cP
<br>@Temperature 536 - 536 °F
Average value: 190000 cP Grade Count:2
190000 - 190000 cP
<br>@Shear Rate 1000 - 1000 1/s
190000 - 190000 cP
<br>@Shear Rate 1000 - 1000 1/s
Average value: 190000 cP Grade Count:2
Viscosity Test 140 - 150 cm³/g
140 - 150 cm³/g
Average value: 144 cm³/g Grade Count:5
Maximum Moisture Content 0.100
0.100
Average value: 0.100 Grade Count:4
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm
0.000300 - 0.0350 in/in
Average value: 0.00391 cm/cm Grade Count:183
0.00300 - 0.00300 cm/cm
<br>@Temperature 80.0 - 80.0 °C
0.00300 - 0.00300 in/in
<br>@Temperature 176 - 176 °F
Average value: 0.00300 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.000700 - 0.0590 cm/cm
0.000700 - 0.0590 in/in
Average value: 0.00787 cm/cm Grade Count:72
0.00600 - 0.00700 cm/cm
<br>@Temperature 80.0 - 80.0 °C
0.00600 - 0.00700 in/in
<br>@Temperature 176 - 176 °F
Average value: 0.00650 cm/cm Grade Count:2
Melt Flow 1.00 - 78.7 g/10 min
1.00 - 78.7 g/10 min
Average value: 32.5 g/10 min Grade Count:22
Spiral Flow 48.0 - 610 cm
18.9 - 240 in
Average value: 163 cm Grade Count:10
Mechanical Properties Metric English Comments
Hardness, Rockwell L 112
112
Average value: 112 Grade Count:3
Hardness, Rockwell M 88.0 - 100
88.0 - 100
Average value: 92.3 Grade Count:8
Hardness, Rockwell R 109 - 124
109 - 124
Average value: 121 Grade Count:40
Hardness, Shore D 77.0 - 91.0
77.0 - 91.0
Average value: 82.5 Grade Count:5
Ball Indentation Hardness 84.0 - 250 MPa
12200 - 36300 psi
Average value: 180 MPa Grade Count:22
Tensile Strength, Ultimate 85.0 - 237 MPa
12300 - 34400 psi
Average value: 166 MPa Grade Count:185
77.0 - 281.306 MPa
<br>@Temperature -40.0 - 150 °C
11200 - 40800.1 psi
<br>@Temperature -40.0 - 302 °F
Average value: 104 MPa Grade Count:4
97.5 - 102.5 MPa
<br>@Temperature 130 - 175 °C
14100 - 14870 psi
<br>@Temperature 266 - 347 °F
Average value: 104 MPa Grade Count:2
97.5 - 102.5 MPa
<br>@Time 1.80e+7 - 7.20e+7 sec
14100 - 14870 psi
<br>@Time 5000 - 20000 hour
Average value: 104 MPa Grade Count:2
40.0 - 160 MPa
<br>@Strain 1.00 - 9.00 %
5800 - 23200 psi
<br>@Strain 1.00 - 9.00 %
Average value: 104 MPa Grade Count:1
40.0 - 160 MPa
<br>@Temperature 60.0 - 150 °C
5800 - 23200 psi
<br>@Temperature 140 - 302 °F
Average value: 104 MPa Grade Count:1
Tensile Strength, Yield 105 - 234 MPa
15200 - 34000 psi
Average value: 180 MPa Grade Count:55
Elongation at Break 1.00 - 11.0 %
1.00 - 11.0 %
Average value: 3.66 % Grade Count:201
2.60 - 7.00 %
<br>@Temperature -40.0 - 150 °C
2.60 - 7.00 %
<br>@Temperature -40.0 - 302 °F
Average value: 5.09 % Grade Count:3
Elongation at Yield 2.00 - 9.50 %
2.00 - 9.50 %
Average value: 3.84 % Grade Count:25
Modulus of Elasticity 1.31 - 15.9 GPa
190 - 2300 ksi
Average value: 9.89 GPa Grade Count:162
2.086 - 12.28 GPa
<br>@Temperature -40.0 - 200 °C
302.6 - 1781 ksi
<br>@Temperature -40.0 - 392 °F
Average value: 7.14 GPa Grade Count:5
Flexural Yield Strength 110 - 352 MPa
16000 - 51100 psi
Average value: 253 MPa Grade Count:152
138 - 450 MPa
<br>@Temperature -40.0 - 121 °C
20000 - 65300 psi
<br>@Temperature -40.0 - 250 °F
Average value: 249 MPa Grade Count:5
Flexural Modulus 1.18 - 13.8 GPa
171 - 2000 ksi
Average value: 9.49 GPa Grade Count:167
4.83 - 12.4795 GPa
<br>@Temperature -40.0 - 121 °C
701 - 1810.03 ksi
<br>@Temperature -40.0 - 250 °F
Average value: 6.81 GPa Grade Count:5
Compressive Yield Strength 149 - 258 MPa
21600 - 37400 psi
Average value: 184 MPa Grade Count:12
Poissons Ratio 0.350
0.350
Average value: 0.350 Grade Count:3
Shear Modulus 4.60 - 5.00 GPa
667 - 725 ksi
Average value: 4.73 GPa Grade Count:3
Izod Impact, Notched 0.427 - 3.68 J/cm
0.800 - 6.90 ft-lb/in
Average value: 1.51 J/cm Grade Count:86
1.91 - 5.12544 J/cm
<br>@Temperature -40.0 - 121 °C
3.58 - 9.60205 ft-lb/in
<br>@Temperature -40.0 - 250 °F
Average value: 1.85 J/cm Grade Count:3
0.74746 - 1.28136 J/cm
<br>@Temperature -40.0 - -40.0 °C
1.4003 - 2.40051 ft-lb/in
<br>@Temperature -40.0 - -40.0 °F
Average value: 1.85 J/cm Grade Count:3
0.74746 - 1.28136 J/cm
<br>@Thickness 3.17 - 3.17 mm
1.4003 - 2.40051 ft-lb/in
<br>@Thickness 0.125 - 0.125 in
Average value: 1.85 J/cm Grade Count:3
Izod Impact, Unnotched 1.33 - 14.4 J/cm
2.50 - 27.0 ft-lb/in
Average value: 10.8 J/cm Grade Count:39
Izod Impact, Notched (ISO) 7.10 - 79.0 kJ/m²
3.38 - 37.6 ft-lb/in²
Average value: 18.9 kJ/m² Grade Count:57
10.0 - 27.0 kJ/m²
<br>@Temperature -40.0 - -20.0 °C
4.76 - 12.8 ft-lb/in²
<br>@Temperature -40.0 - -4.00 °F
Average value: 13.5 kJ/m² Grade Count:21
Izod Impact, Unnotched (ISO) 11.0 - 90.0 kJ/m²
5.23 - 42.8 ft-lb/in²
Average value: 73.9 kJ/m² Grade Count:16
10.0 - 90.0 kJ/m²
<br>@Temperature -30.0 - -30.0 °C
4.76 - 42.8 ft-lb/in²
<br>@Temperature -22.0 - -22.0 °F
Average value: 63.5 kJ/m² Grade Count:6
Charpy Impact Unnotched 3.50 J/cm² - NB
16.7 ft-lb/in² - NB
Average value: 9.02 J/cm² Grade Count:124
3.30 J/cm² - NB
<br>@Temperature -40.0 - 30.0 °C
15.7 ft-lb/in² - NB
<br>@Temperature -40.0 - 86.0 °F
Average value: 7.76 J/cm² Grade Count:77