Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zhejiang Juner 302-G0 Flammable Resistant and Low Separate Out Mode

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner 302-G0 Flammable Resistant and Low Separate Out Mode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, Frameworks of Deflection Coils, Hi-Pressure Outputs Package, Plugs of Kinescopes Autos and Others: Ignition Systems, Heating Systems, Electricity Distribution Systems, Tail Lights Base, Shells of Ignition Coils, Door Handles, Air-Condition LatticesInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
D792
Water Absorption 0.16 %
0.16 %
23°C•24h; D570
Linear Mold Shrinkage 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
D638
Flexural Strength 80.0 MPa
11600 psi
D790
Flexural Modulus 2.50 GPa
363 ksi
D790
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
IS0179
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
IS0179
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
D696
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
D257
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
D150
Dielectric Strength 20.0 kV/mm
508 kV/in
D149
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
D150