Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.020 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
Across Flow; ISO 2577
Polykemi AB POLYelast TPE Z406 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
Linear Mold Shrinkage 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
FRISETTA Test Method
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
ASTM D955
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant
Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
SABIC PP 674K Polypropylene Copolymer for Injection Molding
Product Description: PP 674K is specially developed for producing injection molded & ISBM articles with high clarity and also has better impact properties than homo PP counterparts.PP 674K has the ..
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
FRISETTA Test Method
Nilit FRIANYL C73 M-HS3005 Nylon 6.6/6 for injection molding, 30% mineral filled
Nylon 6.6/6 for injection molding, medium viscosity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Linear Mold Shrinkage 0.013 - 0.020 cm/cm
0.013 - 0.020 in/in
Lehmann & Voss LUVOCOM® 19-8043 Polyamide 46, with PTFE, lubricant modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
Lehmann & Voss LUVOCOM® 1-7830 Polyamide 66, with PTFE, lubricant modified, improved wear resistance, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Linear Mold Shrinkage 0.017 - 0.020 cm/cm
0.017 - 0.020 in/in
ASTM D955
Samyang Triel® 5552EM Thermoplastics Polyetherester Elastomer, Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5552EM is an extrusion grade.Information provided by Samyang.
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Borealis BD310MO Polypropylene Copolymer
BD310MO is a heterophasic copolymer. This grade is characterized by an optimum combination of good impact strength and very high stiffness. This grade is mildly nucleated to maximize the mechanical..
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Borealis BD950MO Polypropylene Copolymer
BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability..
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications
Bormed HF855MO is a high modulus polypropylene homopolymer and is especially developed within the proprietary Borstar technology. Bormed HF855MO combines an unique balance of properties for high sp..
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Borealis Borpact™ SG910MO Polypropylene for Injection Molding
Borpact™ SG910MO is a high impact and transparent polypropylene. This grade provides high gloss, high transparency and excellent impact properties. Applications: containers and products with medium..
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Borealis HD120MO Polypropylene
HD120MO is a polypropylene homopolymer with a good combination of mechanical properties intended for injection molding. Applications: sanitary equipment, caps and closures, and general packagingInf..
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
Borealis MG9621S Polyethylene
MG9621S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 3.20 mm
0.014 - 0.020 in/in

@Thickness 0.126 in
ASTM D 955
RTP Company RTP 100 FR UV Polypropylene (PP) Flame Retardant - Non-PBDE/PBB
Linear Mold Shrinkage 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
D955
Zhejiang Juner 302-G0 Flammable Resistant and Low Separate Out Mode
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Linear Mold Shrinkage 0.015 - 0.020 cm/cm

@Thickness 3.17 mm
0.015 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 1000 TFE 10 SI 2 Polybutylene Terephthalate (PBT), PTFE Lubricated - Silicone Lubricated
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm

@Thickness 3.17 mm
0.0080 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 200 A HS MS Nylon 6 (PA), Molybdenum Disulfide - Heat Stabilized
Linear Mold Shrinkage 0.0020 - 0.020 cm/cm
0.0020 - 0.020 in/in
ASTM D955
Cheng Yu Plastic NG1600S Nylon 66, 60% Glass Fiber Reinforced
Linear Mold Shrinkage 0.0050 - 0.020 cm/cm
0.0050 - 0.020 in/in
ASTM D955
Cheng Yu Plastic T888G15 PBT, 15% Glass Fiber
Linear Mold Shrinkage 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
CPT C-Flex® R70-026 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm
0.0080 - 0.020 in/in
ELASTO UK Dryflex® 400501S SBS Based Material, 50A Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm
0.0080 - 0.020 in/in
ELASTO UK Dryflex® 500800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm
0.0080 - 0.020 in/in
ELASTO UK Dryflex® 662500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm
0.0080 - 0.020 in/in
ELASTO UK Dryflex® 662650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Linear Mold Shrinkage 0.0020 - 0.020 cm/cm
0.0020 - 0.020 in/in
ASTM D955
Cheng Yu Plastic FR200N Flame Retardant Nylon 66
Linear Mold Shrinkage 0.017 - 0.020 cm/cm
0.017 - 0.020 in/in
after bake; ISO 294
Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene  (discontinued **)
Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers. LyondellBasel..
Linear Mold Shrinkage 0.015 - 0.020 cm/cm

@Thickness 3.17 mm
0.015 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 151 HF Polypropylene (PP), High Flow - Flame Retardant - Halogen Free
Linear Mold Shrinkage 0.013 - 0.020 cm/cm
0.013 - 0.020 in/in
ASTM D955
Chang Chun Plastic PBT2100 Fire Retardant PBT
Information provided by Dowell Trading Company Ltd.
Linear Mold Shrinkage 0.017 - 0.020 cm/cm
0.017 - 0.020 in/in
ASTM D955
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5700 is an extrusion grade.Information provided by Samyang.