Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 56.5 MPa | 8190 psi | ASTM D882 |
ExxonMobil LL 1002.32 Cast Film Resin
(discontinued **) LL 1002.32 is a butene LLDPE resin designed for the cast film process. Films made from LL 1002.32 have very good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, MD | 56.5 MPa | 8200 psi | ASTM D882 |
Westlake Hifor Clear SC74580 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It doe.. |
|||
Film Tensile Strength at Break, MD | 56.5 MPa | 8200 psi | ASTM D882 |
Westlake Mxsten CV77516 Polyethylene Plastomer Mxsten CV Plastomer CV77516 resin is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a very low se.. |
|||
Film Tensile Strength at Break, MD | 56.5 MPa | 8190 psi | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Film Tensile Strength at Break, MD | 56.5 MPa | 8190 psi | |
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati.. |
|||
Film Tensile Strength at Break, MD | 56.5 MPa | 8190 psi | |
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food .. |
|||
Film Tensile Strength at Break, MD | 56.5 MPa | 8200 psi | ASTM D882 |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |