Material Notes:
Injection Molding Grade. Heat Stabilized. Meets Ford ESH-M4D293-B Spec.Data provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 25 - 40 g/10 min
25 - 40 g/10 min
Cond L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
Secant; ASTM D790
Izod Impact, Notched 0.700 J/cm

@Thickness 3.17 mm
1.31 ft-lb/in

@Thickness 0.125 in
ASTM D256
Gardner Impact 15.0 J
11.1 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ASTM D256