Melt Flow 30 - 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 - 40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1452S (H39S) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 30 - 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 - 40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1548S (H32GA) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 20 - 40 g/10 min

@Load 3.80 kg,
Temperature 300 °C
20 - 40 g/10 min

@Load 8.38 lb,
Temperature 572 °F
ASTM D1238
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy
Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Melt Flow 15 - 40 g/10 min
15 - 40 g/10 min
ASTM D1238
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade
Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 15 - 40 g/10 min

@Load 11.6 kg,
Temperature 250 °C
15 - 40 g/10 min

@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
Melt Flow 20 - 40 g/10 min

@Load 11.6 kg,
Temperature 250 °C
20 - 40 g/10 min

@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Melt Flow 20 - 40 g/10 min
20 - 40 g/10 min
ASTM D1238
Polymer Resources PPX-FR2-[color]EN Modified PPO, UL 94 V-1 with HDT of 210 F, Extrusion Grade
Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 20 - 40 g/10 min

@Load 11.6 kg,
Temperature 250 °C
20 - 40 g/10 min

@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
Polymer Resources PPX-FR2-[color]-EN Modified-PPO, V-1 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
Melt Flow 15 - 40 g/10 min

@Load 2.16 kg,
Temperature 170 °C
15 - 40 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane
Pearlbond® 12C75 is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softe..
Melt Flow 20 - 40 g/10 min

@Load 2.16 kg,
Temperature 150 °C
20 - 40 g/10 min

@Load 4.76 lb,
Temperature 302 °F
Taiwan Sheen Soon Sheenthane® AH-591 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Melt Flow 34 - 40 g/10 min

@Load 5.00 kg,
Temperature 365 °C
34 - 40 g/10 min

@Load 11.0 lb,
Temperature 689 °F
ASTM D1238
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
Melt Flow 30 - 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 - 40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF)
Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope..
Melt Flow 15 - 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 - 40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
DIN 53735
Stanelco Bioplast® GS 2189 Biodegradable Plastic
Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i..
Melt Flow 20 - 40 g/10 min

@Load 21.6 kg,
Temperature 190 °C
20 - 40 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Melt Flow 20 - 40 g/10 min

@Load 21.6 kg,
Temperature 190 °C
20 - 40 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol.
Melt Flow 15 - 40 g/10 min

@Load 8.70 kg,
Temperature 215 °C
15 - 40 g/10 min

@Load 19.2 lb,
Temperature 419 °F
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Melt Flow 20 - 40 g/10 min

@Load 21.6 kg,
Temperature 190 °C
20 - 40 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Melt Flow 16 - 40 g/10 min

@Load 5.00 kg,
Temperature 232 °C
16 - 40 g/10 min

@Load 11.0 lb,
Temperature 450 °F
ASTM D1238
Arkema Group KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Melt Flow 30 - 40 g/10 min
30 - 40 g/10 min
ASTM D359
Asahi Glass Fluon® LM-740AP LM-ETFE Fluororesin
Fluon®LM-ETFE combines the excellent properties in heat resistance and other mechanical properties owned by ETFE resin and the low melting point.Information provided by Asahi Glass Company, Inc.
Melt Flow 20 - 40 g/10 min
20 - 40 g/10 min
ASTM D1238
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 20 - 40 g/10 min
20 - 40 g/10 min
ASTM D1238
Polymer Resources PPX-FR2 Modified PPO, UL 94 V-1 with HDT of 210 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 25 - 40 g/10 min
25 - 40 g/10 min
Cond L; ASTM D1238
Washington Penn PPC7UF0-Black Polypropylene, High Flow Copolymer
Injection Molding Grade. Heat Stabilized. Meets Ford ESH-M4D293-B Spec.Data provided by Washington Penn Plastic Co., Inc.
Melt Flow 20 - 40 g/10 min

@Load 8.70 kg,
Temperature 205 °C
20 - 40 g/10 min

@Load 19.2 lb,
Temperature 401 °F
Lubrizol Estane® GP 52 DT Thermoplastic Polyurethane
Type: Estane® GP 52DT is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E..