Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2EU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol B120MA Polypropylene REPOL Polypropylene B120MA is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 0.700 - 1.60 J/cm | 1.31 - 3.00 ft-lb/in | Average value: 1.03 J/cm Grade Count:3 |
Overview of materials for Nylon 6/69 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256/ISO 180 |
Ineos Styrenics Polystyrene 147F (NAFTA) An easy flow, general purpose polystyrene. Has moderate heat resistance and strength for general molding and extrusion applications.Information provided by BASF.Ineos Styrenics purchased this produ.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | 23° C; ASTM D256 |
Flint Hills P5M4K-046 Random Copolymer Polypropylene Random copolymer, FDA compliant.Features: Clarified (50 mil plaque haze 10%), antistat, and controlled rheology.Applications: Injection molding: high clarity parts, medical parts, and good organolep.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM DH1004 PEI |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem DH1004F PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 0.000 °C |
1.31 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 Conductive GTX, CTE 7 |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature -30.0 °C |
1.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | |
UBE UBEPOL BR15H HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBEPOL-BR15H is a in-between polymer of UBEPOL-BR15HB and UBEPOL-BR15HL.Information provided by UBE. |
|||
Izod Impact, Notched | 0.700 J/cm @Temperature 23.0 °C |
1.31 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA301G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.700 - 1.10 J/cm @Temperature -40.0 - -40.0 °C |
1.31 - 2.06 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.900 J/cm Grade Count:2 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® R-7 02 Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® R-7 02 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound wit.. |
|||
Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Asia Pacific) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |