Polymer Property : 300% Modulus = 1.02 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00700 GPa
1.02 ksi
DIN 53504
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 70 H 4673 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4673 M is part of the HUNTSMAN injection molding ..
300% Modulus 0.00700 GPa
1.02 ksi
0.025" extruded film; DIN 53504
Huntsman IROGRAN® A 70 H 4714 M TPU-Polyester
Introduction: IROGRAN A 70 H 4714 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4714 M is part of the HUNTSMAN injection molding ..
300% Modulus 0.00700 GPa
1.02 ksi
ISO 527
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane
Pearlbondâ„¢ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus..
300% Modulus 0.00700 GPa
1.02 ksi
ISO 37
Huntsman AVALON® 75 AE Thermoplastic Polyurethane
Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material ..
300% Modulus 0.00700 GPa
1.02 ksi
ISO 527
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low soft..
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-A880 Aliphatic TPU
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.00700 GPa
1.02 ksi
ISO 37
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D638
ELASTO UK Dryflex® 400901S SBS Based Material, 90A Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D638
ELASTO UK Dryflex® 402901S SBS Based Material, 90A Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D638
ELASTO UK Dryflex® 500900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D638
ELASTO UK Dryflex® 502900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D638
ELASTO UK Dryflex® 660900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D638
ELASTO UK Dryflex® 662900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00700 GPa
1.02 ksi
ASTM D 638
API Megol AM DP2395/85 SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..