SABIC Innovative Plastics LNP Thermocomp 2FL24 FP-E (EFTE)

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp 2FL24 FP-E (EFTE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* 2FL24 is a Fluoropolymer, ETFE grade containing Glass Fibers and PTFE.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
ASTM D 792
Density 1.80 g/cc
0.0650 lb/in³
ASTM D 792
Moisture Absorption at Equilibrium 0.010 %
0.010 %
23°C / 50% RH; ISO 62
0.00 %

@Time 86400 sec
0.00 %

@Time 24.0 hour
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm

@Time 86400 sec
0.010 - 0.030 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 67.0 MPa
9720 psi
5 mm/min; ISO 527
69.0 MPa
10000 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 6.2 %
6.2 %
5 mm/min; ISO 527
6.5 %
6.5 %
Type I, 5 mm/min; ASTM D 638
Tensile Modulus 5.00 GPa
725 ksi
1 mm/min; ISO 527
6.44 GPa
934 ksi
5 mm/min; ASTM D 638
Flexural Strength 89.0 MPa
12900 psi
ISO 178
Flexural Modulus 4.76 GPa
690 ksi
1.3 mm/min, 50 mm span; ASTM D 790
4.98 GPa
722 ksi
2 mm/min; ISO 178
Izod Impact, Notched 4.88 J/cm

@Temperature 23.0 °C
9.14 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 13.4 J/cm

@Temperature 23.0 °C
25.1 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 92.0 kJ/m²

@Temperature 23.0 °C
43.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 8.00 J
5.90 ft-lb
Multiaxial Impact; ISO 6603
20.0 J

@Temperature 23.0 °C
14.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 24.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
52.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
Deflection Temperature at 0.46 MPa (66 psi) 239 °C
462 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
251 °C

@Thickness 3.20 mm
484 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
198 °C

@Thickness 3.20 mm
388 °F

@Thickness 0.126 in
unannealed; ASTM D 648