Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00700 GPa | 1.02 ksi | DIN 53504 |
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 70 H 4673 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4673 M is part of the HUNTSMAN injection molding .. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | 0.025" extruded film; DIN 53504 |
Huntsman IROGRAN® A 70 H 4714 M TPU-Polyester Introduction: IROGRAN A 70 H 4714 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4714 M is part of the HUNTSMAN injection molding .. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ISO 527 |
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane Pearlbond™ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus.. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ISO 37 |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ISO 527 |
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane Pearlbond™ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low soft.. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-A880 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ISO 37 |
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D638 |
ELASTO UK Dryflex® 400901S SBS Based Material, 90A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D638 |
ELASTO UK Dryflex® 402901S SBS Based Material, 90A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D638 |
ELASTO UK Dryflex® 500900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D638 |
ELASTO UK Dryflex® 502900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D638 |
ELASTO UK Dryflex® 660900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D638 |
ELASTO UK Dryflex® 662900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00700 GPa | 1.02 ksi | ASTM D 638 |
API Megol AM DP2395/85 SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |