Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.793 GPa | 115 ksi | 2% Strain; ASTM D 638 type IV |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Secant Modulus | 0.793 GPa | 115 ksi | 2% Strain; ASTM D 638 type IV |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Secant Modulus | 0.793 GPa | 115 ksi | ASTM D882 |
Total PPH 3571 Polypropylene, Film Extrusion Grade Homopolymer film gradeLow Residuals - Fina 3571 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina.. |
|||
Secant Modulus | 0.793 GPa | 115 ksi | ASTM D882 |
Total PPH 3576XHD Polypropylene Homopolymer, Film Grade Low Residuals TOTAL Polypropylene 3576XHD utilizes the new ATOFINA proprietary process technology to provide extremely low residuals for improved color stability and clarity.Antiblock. 3576XHD is .. |