Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total HDPE MS201 BN-NA High Density Polyethylene - Fuel Tank Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Total Atofina
Trade Name HDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total HDPE MS201 BN-NA High Density Polyethylene - Fuel Tank Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyethylene: High molecular weight, high density fuel tank resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceGMP.PE.062 certification.Applications: Automotive fuel tanksInformation provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.946 g/cc
0.946 g/cc
ISO 1183
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693
Melt Flow 6.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527
Elongation at Break >= 600 %
>= 600 %
ISO 527
Flexural Modulus 1.10 GPa

@Strain <=0.400 %
160 ksi

@Strain <=0.400 %
ISO 178
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 127 °C
260 °F
ASTM D3417
Processing Properties Metric English Comments
Processing Temperature 188 - 232 °C
370 - 450 °F
Blow Molding Stock Temp.