Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.946 - 0.956 g/cc | 0.946 - 0.956 g/cc | ASTM D792 |
Ravago Manufacturing Americas Echo® RPEHD NAT Recycled HDPE Recycled High Density Polyethylene, Natural Color, Fractional Melt FlowInformation provided by Ravago. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D1505 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D1505 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D1505 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D792 |
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ISO 1183 |
Total HDPE MS201 BN-NA High Density Polyethylene - Fuel Tank Resin Polyethylene: High molecular weight, high density fuel tank resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceGMP.PE.062 certification.Appl.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D1505 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D792 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D1505 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | |
Dow Corning Z-6011 SILANE Dow Corning® Z-6011 Silane is a reactive chemical containing an aminopropyl organic group and a triethoxysilyl inorganic group. Chemically, Dow Corning® Z-6011 Silane is designated gammaaminopropy.. |
|||
Specific Gravity | 0.946 g/cc | 0.946 g/cc | ASTM D1505 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |