Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Evatane® 24 - 03 HDPE vinyl acetate copolymer, blown film, injection molding  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Evatane® 24 - 03 HDPE vinyl acetate copolymer, blown film, injection molding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ISO 1183
Melt Flow 2.0 g/10 min
2.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 30
30
ISO 868
Tensile Strength at Break 29.0 MPa
4210 psi
ISO 527
Elongation at Break 750 %
750 %
ISO 527
Modulus of Elasticity 0.0350 GPa
5.08 ksi
ISO 5527
Dart Drop Test >= 1000 g
>= 2.20 lb
50µ; ISO 7765-1
Thermal Properties Metric English Comments
Melting Point 77.0 °C
171 °F
ISO 11357-3
Vicat Softening Point 52.0 °C
126 °F
ISO 306
Descriptive Properties Value Comments
Food Status This material conforms to both European and American Food contact regulations.